Sign In | Join Free | My carsrow.com
China SKYLINE INSTRUMENTS CO.,LTD logo
SKYLINE INSTRUMENTS CO.,LTD
Skyline Instruments Co.,LTD We only manufacture Lab Testing Equipment
Verified Supplier

10 Years

Home > Lab Testing Equipment >

SL-P05 DSC100A Differential Scanning Calorimeter

SKYLINE INSTRUMENTS CO.,LTD
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

SL-P05 DSC100A Differential Scanning Calorimeter

Model Number : SL-P05

MOQ : 1

Delivery Time : 25 working days

Place of Origin : China

Payment Terms : L/C,D/A,D/P,T/T,Western Union

Supply Ability : 15 sets/month

Certification : CE, CO, Rosh, Form E, Calibrate Certificate

Brand Name : SKYLINE

Price : Negotiable

Packaging Details : Standard Export Package

Contact Now

SL-P05 DSC100A Differential Scanning Calorimeter
SL-P05 DSC100A Differential Scanning Calorimeter
Applications
The DSC100A is among the most accurate differential scanning calorimeter models available. It features a highly sensitive E-pair sensor made from imported materials, shielded signal acquisition circuitry for strong interference resistance, and exceptional baseline stability.
This touch screen differential scanning calorimeter performs comprehensive thermal analysis including glass transition temperature testing, phase transition analysis, melting and enthalpy measurements, product stability assessment, curing studies, oxidation induction period testing, and oxidation induction temperature determination.
Compliance Standards
  • GB/T 19466.2-2004 / ISO 11357-2:1999 - Determination of glass transition temperature
  • GB/T 19466.3-2004 / ISO 11357-3:1999 - Determination of melting and crystallization temperatures and enthalpy
  • GB/T 19466.6-2009 / ISO 11357-6:1999 - Oxidation induction period determination (isothermal OIT) and oxidation induction temperature (dynamic OIT)
Technical Specifications
Temperature range: Room temperature ~600°C (air cooling)
Temperature resolution: 0.01°C
Temperature fluctuation: ±0.1°C
Temperature repeatability: ±0.1°C
Heating rate: 0.1 ~ 100°C/min
Data scanning: Temperature scanning
Temperature control mode: Temperature rise, constant temperature (automatic program control)
DSC range: 0 ~ ±600mW
DSC resolution: 0.01μW
DSC sensitivity: 0.001mW
Power supply: AC220V/50Hz or customized
Atmosphere control gas: Nitrogen, oxygen (automatic instrument switching)
Gas flow rate: 0-300mL/min
Gas pressure: 0.2MPa
Display mode: 24bit color, 7 inch LCD touch screen display
Data interface: Standard USB interface
The instrument includes standard calibration materials (indium, tin) for user temperature adjustment. The integrated software platform supports thermogravimetric and synchronous instruments. Multiple thermocouple sets monitor sample temperature and internal instrument temperature separately.
Key Features
  • Industrial-grade 7-inch touch screen with comprehensive information display
  • Advanced metal furnace structure delivers superior baseline performance and higher precision
  • Indirect conduction heating provides exceptional uniformity and stability while reducing pulse radiation
  • USB communication interface ensures reliable data transfer with self-recovery functionality
  • Automatic dual-gas flow switching with rapid stabilization and protective gas input
  • Intuitive, user-friendly software interface
Furnace Construction
SL-P05 DSC100A Differential Scanning Calorimeter
Software Interface
SL-P05 DSC100A Differential Scanning Calorimeter SL-P05 DSC100A Differential Scanning Calorimeter

Product Tags:

DSC100A differential scanning calorimeter

      

SL-P05 lab testing equipment

      

DSC100A thermal analysis instrument

      
 SL-P05 DSC100A Differential Scanning Calorimeter Manufactures

SL-P05 DSC100A Differential Scanning Calorimeter Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: SKYLINE INSTRUMENTS CO.,LTD
*Subject:
*Message:
Characters Remaining: (0/3000)